| TIG-NiCrMo3 |
Classifications: GB/T15620 SNi6625 AWS A5.14 ERNiCrMo-3 AWS A5.14M ERNiCrMo-3 ISO 18274:S Ni 6625 |
|||||||||||||||||||||
| TIG solid rod for nickel alloy | ||||||||||||||||||||||
| NiCrMo type / For Inconel 625 alloy | ||||||||||||||||||||||
| Approval: | ||||||||||||||||||||||
| ABS, BV | ||||||||||||||||||||||
| Application: | ||||||||||||||||||||||
|
Suitable for welding Ni-Cr-Mo alloy, such as lnconel 625, Incoloy 825, can be used for dissimilar metal welding and buildup welding with nickel alloy and stainless steel, can be used in environment between low temperature to 540℃ |
||||||||||||||||||||||
| Characteristics: | ||||||||||||||||||||||
|
1. Ni-Cr-Mo type nickel alloy argon gas shielding TIG rod, nominal composition is: 61%Ni-22%Cr-9%Mo-3.5%Nb+Ta; 2. Deposited metal with excellent mechanical properties and pitting resistance and crevice corrosive resistance; 3. Stable arc, beautiful weld bead appearance, great iron water fluidity, excellent weldability. |
||||||||||||||||||||||
| Polarity: | ||||||||||||||||||||||
| DC- | ||||||||||||||||||||||
| Welding Position: | ||||||||||||||||||||||
|
|
|
|
|
|
|||||||||||||||||
| Typical Chemical Composition of Weld Metal: | ||||||||||||||||||||||
| Alloy wt% | C | Mn | Si | Cr | Ni | Mo | Fe | Nb+Ta | P | S | ||||||||||||
| GB/T | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58.0 | 8.0-10.0 | 5.0 | 3.0-4.2 | - | - | ||||||||||||
| AWS | 0.10 | 0.50 | 0.50 | 20.0-23.0 | ≥58.0 | 8.0-10.0 | 5.0 | 3.15-4.15 | 0.02 | 0.015 | ||||||||||||
| EXP | 0.005 | 0.17 | 0.13 | 21.94 | 64.82 | 8.77 | 0.17 | 3.50 | 0.002 | 0.003 | ||||||||||||
| Typical Mechanical Properties of Weld Metal: | ||||||||||||||||||||||
|
Mechanica properties |
Y.S.(MPa) | T.S.(MPa) | EI(%) | CVN(J/℃) | FN | |||||||||||||||||
| YB/T | - | - | - | - | - | |||||||||||||||||
| AWS | - | 760 | - | - | - | |||||||||||||||||
| EXP | - | 790 | 45 | 162/-196 | - | |||||||||||||||||
| Notes on usage: | ||||||||||||||||||||||
|
1. Shielding gas: Pure Ar; 2. Interpass temperature: <=100℃. The above recommendation is for your reference, actual operation depends on the conditions on site; when necessary, prepare WPS first before deciding the corresponding welding methods. |
||||||||||||||||||||||