TIG-317L/ER317L

TIG-317L Classification:
YB/T5092 H022Cr19Ni14Mo3
AWS A5.9 ER317L
AWS A5.9M ER317L
ENISO14343-A: W(18 15 3 L)
ENISO14343-B: SS317L
Stainless Steel TIG Solid Wire
Austenitic Alloy
Approval:
CE
Application:
For joining 19Cr-13Ni-3Mo(SUS317) grade stainless austenitic steels used in fertilizer production, storage tanks and other structures where high corrosion resistance properties are required.
Characteristics:
1.Weld deposits have excellent mechanical properties and high corrosion resistance;
2.Stable arc, less spattering,good bead appearance.
Polarity:
DC-
Welding Position:
Typical Chemical Composition of Weld Metal:
Alloy wt% C Mn Si Cr Ni Mo P S Cu
YB/T 0.03 1.0-2.5 0.65 18.5-20.5 13.0-15.0 3.0-4.0 0.03 0.030 0.75
AWS 0.03 1.0-2.5 0.30-0.65 18.5-20.5 13.0-15.0 3.0-4.0 0.03 0.030 0.75
EXP 0.016 1.58 0.54 19.32 13.58 3.24 0.015 0.008 0.07
Typical Mechanical Properties of Weld Metal:
Mechanica
properties
Y.S.(MPa) T.S.(MPa) EI(%) CVN(J/℃) PWHT(℃xh)
YB/T - - - - -
AWS - - - - -
EXP - 600 37 - -
Notes on usage:
1. Shielding gas: 100% Ar;
2.Shielding gas flow rate: 10-15 l/min;
3. Arc length should be kept between 1-3 mm;
4.Interpass temperature: ≤150℃;
5. Prior to welding, base metal surfaces should be cleaned of grease, oil and corrosion contamination;
6. Take proper protection against wind to prevent blowholes when welding outdoors.